Still deciding? Get samples of $ !
Request Sample
|
| Customization: | Available |
|---|---|
| Antistatic Properties: | High Antistatic |
| Breathability: | High |
| Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
|---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency

Product feature:
Built-in conductive yarn, permanent stable anti-static effect
Polyester/poly-cotton material, breathable and wear-resistant
Lint-free, low dust, fit for clean room use
Repeated washable, no performance decline
Good color fastness, not easy to fade or deform
Various weights, colors and widths in stock
Meet industry ESD standards, test reports available
| Item | Standard |
Testing methods or tools
|
|
Point to point resistance
|
≤10e6 ohms
(strip: longitude)
(grid: longitude and latitude)
|
GB12014-2019
|
| PH |
4.0~8.5
|
GB/T 7573-2009 0.1mol/L KCl solution
|
|
Formaldehyde content (mg/kg)
|
≤75
|
GB/T 2912.1-2009 Water extraction method
|
|
Color fastness to light (grade)
|
≥3-4
|
GB/T 8427-2008 Method 3
|
|
Color fastness to dry rubbing (grade)
|
≥3-4 |
GB/T 3920-2008
|
|
Color fastness to washing (grade)
|
Discoloration ≥3-4
Color staining ≥3-4
|
GB/T 3921-2008 A(1) 40ºC
|
|
Dimensional change after washing
|
Warp: ±2.5%
Weft: ±2.5%
|
GB/T8629-2017 A-type washing machine
Program 4N, hang to dry.
|
|
Breaking strength
|
Warp ≥400N
Weft ≥400N
|
GB/T 3923.1-2013 Determination of breaking
strength and elongation at break (strip method
|
|
Tearing strength
|
Longitudinal direction ≥15N
Latitude direction ≥15N
|
GB/T 3917.3-2009 Determination of tearing
strength of trapezoidal specimens
|